Stainless Steel Rod Ultra Manipis na Metal Wire
Panimula Sa Steel Wire
Grado ng bakal: Bakal
Mga Pamantayan: AISI, ASTM, BS, DIN, GB, JIS
Pinagmulan: Tianjin, China
Uri: Bakal
Application: pang-industriya, pagmamanupaktura ng mga fastener, nuts at bolts, atbp
Haluang metal o hindi: hindi haluang metal
Espesyal na layunin: libreng pagputol ng bakal
Modelo: 200, 300, 400, serye
Pangalan ng tatak: zhongao
Grado: hindi kinakalawang na asero
Sertipikasyon: ISO
Nilalaman (%): ≤ 3% Si content (%): ≤ 2%
Wire gauge: 0.015-6.0mm
Sample: magagamit
Haba: 500m-2000m / reel
Ibabaw: maliwanag na ibabaw
Mga katangian: paglaban sa init
Stainless steel wire drawing (stainless steel wire drawing): isang metal plastic processing process kung saan ang wire rod o wire blank ay kinukuha mula sa die hole ng wire drawing die sa ilalim ng pagkilos ng drawing force para makagawa ng small-section steel wire o isang non-ferrous na metal wire.Ang mga wire na may iba't ibang cross-sectional na hugis at sukat ng iba't ibang mga metal at haluang metal ay maaaring gawin sa pamamagitan ng pagguhit.Ang iginuhit na wire ay may mga tumpak na sukat, makinis na ibabaw, simpleng kagamitan sa pagguhit at mga hulma, at madaling pagmamanupaktura.
Pagpapakita ng Produkto
Mga Katangian ng Proseso
Ang stress state ng wire drawing ay ang three-dimensional na principal stress state ng two-way compressive stress at one-way tensile stress.Kung ikukumpara sa principal stress state kung saan ang lahat ng tatlong direksyon ay compressive stress, ang iginuhit na metal wire ay mas madaling maabot ang estado ng plastic deformation.Ang deformation state ng drawing ay isang three-way na pangunahing deformation state ng two-way compression deformation at isang tensile deformation.Ang estado na ito ay hindi mabuti para sa plasticity ng mga metal na materyales, at mas madaling makagawa at ilantad ang mga depekto sa ibabaw.Ang dami ng pass deformation sa proseso ng pagguhit ng wire ay limitado sa pamamagitan ng safety factor nito, at mas maliit ang halaga ng pass deformation, mas maraming pass ang drawing.Samakatuwid, ang maramihang mga pass ng tuloy-tuloy na high-speed drawing ay kadalasang ginagamit sa paggawa ng wire.
Saklaw ng Wire Diameter
Wire diameter(mm) | Xu tolerance(mm) | Pinakamataas na diameter ng deviation(mm) |
0.020-0.049 | +0.002 -0.001 | 0.001 |
0.050-0.074 | ±0.002 | 0.002 |
0.075-0.089 | ±0.002 | 0.002 |
0.090-0.109 | +0.003 -0.002 | 0.002 |
0.110-0.169 | ±0.003 | 0.003 |
0.170-0.184 | ±0.004 | 0.004 |
0.185-0.199 | ±0.004 | 0.004 |
0.-0.299 | ±0.005 | 0.005 |
0.300-0.310 | ±0.006 | 0.006 |
0.320-0.499 | ±0.006 | 0.006 |
0.500-0.599 | ±0.006 | 0.006 |
0.600-0.799 | ±0.008 | 0.008 |
0.800-0.999 | ±0.008 | 0.008 |
1.00-1.20 | ±0.009 | 0.009 |
1.20-1.40 | ±0.009 | 0.009 |
1.40-1.60 | ±0.010 | 0.010 |
1.60-1.80 | ±0.010 | 0.010 |
1.80-2.00 | ±0.010 | 0.010 |
2.00-2.50 | ±0.012 | 0.012 |
2.50-3.00 | ±0.015 | 0.015 |
3.00-4.00 | ±0.020 | 0.020 |
4.00-5.00 | ±0.020 | 0.020 |
Kategorya ng Produkto
Sa pangkalahatan, ito ay nahahati sa 2 serye, 3 serye, 4 na serye, 5 serye at 6 na serye na hindi kinakalawang na asero ayon sa austenitic, ferritic, two-way na hindi kinakalawang na asero at martensitic na hindi kinakalawang na asero.
Ang 316 at 317 na hindi kinakalawang na asero (tingnan sa ibaba para sa mga katangian ng 317 hindi kinakalawang na asero) ay mga hindi kinakalawang na asero na naglalaman ng molibdenum.Ang nilalaman ng molibdenum sa 317 hindi kinakalawang na asero ay bahagyang mas mataas kaysa sa 316 hindi kinakalawang na asero.Dahil sa molibdenum sa bakal, ang pangkalahatang pagganap ng bakal na ito ay mas mahusay kaysa sa 310 at 304 na hindi kinakalawang na asero.Sa ilalim ng mga kondisyon ng mataas na temperatura, kapag ang konsentrasyon ng sulfuric acid ay mas mababa sa 15% at mas mataas sa 85%, 316 Hindi kinakalawang na asero ay may malawak na hanay ng mga gamit.Ang 316 na hindi kinakalawang na asero ay mayroon ding mahusay na pagtutol sa chloride corrosion, kaya kadalasang ginagamit ito sa mga marine environment.Ang 316L na hindi kinakalawang na asero ay may pinakamataas na nilalaman ng carbon na 0.03, na maaaring magamit sa mga aplikasyon kung saan ang pagsusubo ay hindi maaaring isagawa pagkatapos ng hinang at ang pinakamataas na resistensya ng kaagnasan ay kinakailangan